Summary
Objective To heat a stainless steel conduit, ferrule and elbow assembly to 1400F (760C) within 20 seconds for brazing.Material 6”(152.4mm)long x 0.5”(12.7mm) diameter stainless steel conduit, 0.5”(12.7mm) long x 0.5”(12.7mm) diameter ferrule, 2”(50.8m…

Objective To heat a stainless steel conduit, ferrule and elbow assembly to 1400°F (760°C) within 20 seconds for brazing.
Material 6”(152.4mm)long x 0.5”(12.7mm) diameter stainless steel conduit, 0.5”(12.7mm) long x 0.5”(12.7mm) diameter ferrule, 2”(50.8mm) elbow with 0.5” (12.7mm) diameter
Temperature 1400°F (760°C)
Frequency 70 kHz
Equipment •  Power of 15 kW induction heating system equipped with a remote workhead
• An induction heating coil designed and developed specifically for this application.
Process A specially designed, three-turn helical coil is used to provide heat to the assembly at the braze joint area. Two small silver solder braze rings are placed at each joint; the joints are coated with black flux to insure that the braze material flows cleanly. The assembly is placed inside the coil and power is applied for 15 seconds to cause the braze to flow.
Results/Benefits Induction heating provides:
• Consistent and repeatable results
• No flame process
• Faster process time

brazing-steel-Ferrule
brazing-steel-Ferrule

Tags
induction heating, induction heater, induction heating machine, Melting gold, gold melting, induction melting gold, induction gold melting furnace, induction heating equipment, high frequency heating

Newest Comment

    No Comment

Post Comment

Verify Code:
United Induction Heating Machine Limited
© Copyright 2024. uihm.com All Rights Reserved.