Summary
Shrink fitting impeller blades to shaft Objective Heat aluminum impeller blades to 200 F (93 C) and shrink fit onto a shaft.Material Aluminum impeller blades with a .28” (7.109mm) bore, aluminum shaftTemperature 200 F (93 C)Frequency 255 kHzEquipment…
Shrink fitting impeller blades to shaft

Objective Heat aluminum impeller blades to 200 ºF (93 ºC) and shrink fit onto a shaft.
Material Aluminum impeller blades with a .28” (7.109mm) bore, aluminum shaft
Temperature 200 ºF (93 ºC)
Frequency 255 kHz
Equipment • Power of 6 kW induction heating system, equipped with a remote workhead containing one 1.0μF capacitor.
• An induction heating coil designed and developed specifically for this application.
Process A split two turn helical coil is used to evenly heat the opening on the impeller blade. The impeller blade is heated for 20 seconds to reach the 200 ºF (93 ºC). The impeller blades are then removed from the coil & slipped over the shaft to
complete the shrink fitting application.
Results/Benefits Induction heating provides:
• Repeatable results
• Reduced cycle time, lower consumables cost
• Even distribution of heating

Shrink fitting impeller blades to shaft

Shrink fitting impeller blades to shaft

Tags
induction heating, induction heater, induction heating machine, Melting gold, gold melting, induction melting gold, induction gold melting furnace, induction heating equipment, high frequency heating

Newest Comment

    No Comment

Post Comment

Verify Code:
United Induction Heating Machine Limited
© Copyright 2024. uihm.com All Rights Reserved.