Keywords"induction",total 2889 records
-
metal to plastic by induction bonding
Objective To heat a steel magnetic steel post to 300F for a bonding application.Material Magnetic steel posts Plastic handleTemperature indicating paintTemperature 300F (149C)Frequency 288 kHzEquipment Power of 6 kW, 100-400 kHz induction heating power sup…
Date:2007/04/03
-
induction annealing stress relieving
STRESS RELIEVING,NORMALISING AND ANNEALINGStress RelievingStress relieving is applied to both ferrous and non-ferrous alloys and is intended to remove internal residual stresses generated by prior manufacturing processes such as machining, cold rolling and…
Date:2007/04/03
-
induction hardening and flame hardening
WHAT ARE THE TREATMENTS? Induction hardening and flame hardening are methods for hardening the surfaces of components, usually in selected areas, by the short-time application of high-intensity heating followed by quenching. The heating and hardening eff…
Date:2007/04/03
-
induction hardening and tempering of tools
WHAT ARE THE STEELS?Tool and die steels are covered in BS 4659:1989, although both American nomenclature and a variety oftrade names are also in use. Available in high-quality grades, these specifically-designed steels can be groupedbroadly according to t…
Date:2007/04/03
-
induction de-bonding stainless steel
Objective To separate bonded stainless steel / carbon fiber assemblies by heating tang, softening the adhesive bond Material Stainless steel and carbon fiber inserts Temperature 300 F (149C) Frequency 200 kHz Equipment • Power of 6kW induction heating…
Date:2007/04/03
-
induction bonding plastic sleeve to stainless steel handle
Objective Heating end of a stainless steel handle with a plastic sleeve coated with heat adhesive for a bonding applicationMaterial 1” (25mm) OD stainless steel handle 0.30” (7.6) thick covered with a plastic sleeve that is coated with a heat adhesive be…
Date:2007/04/03
-
induction debond rubber seal from steel
Objective Debond a fluorocarbon rubber seal from a carbon steel oil seal Material 4” (10.2cm) OD carbon steel oil seal with a fluorocarbon rubber seal Temperature 1200 F (649 C) Frequency 179 kHz Equipment • Power of 6kW induction heating system, equi…
Date:2007/04/03
-
induction bonding gasket to nut
Objective To heat a steel sombrero nut prior to gasket bonding Material • Steel sombrero-shaped nut approx. 2” (50.8mm) diameter, 2” (50.8mm) in height • gasket Temperature 350 F (176 C) Frequency 266 kHz Equipment • Power of 6kW induction heating…
Date:2007/04/03
-
induction brazing thin walled tube
Objective Braze a NI-SPAN-C alloy tube to a steel cap in a hydrogen atmosphere Material NI-SPAN-C alloy tube (5mm) dia, steel cap (7mm) dia, (7mm) long, nickel braze, quartz tube and hydrogen Temperature 1875 F (1024 C) Frequency 313 kHz Equipment • P…
Date:2007/04/03
-
induction brazing piston valve
Objective Brazing a steel piston valve assembly Material Steel piston valve 4.5” dia (11.43cm), tungsten carbide plate and braze Temperature 1350 F Frequency 91 kHz Equipment • Power of 90kW induction heating system, equipped with a remote workhead c…
Date:2007/04/03