Keywords"Phosphor copper brazing ring",total 302 records
-
induction soldering stainless steel
Soldering stainless steel Objective Heat Stainless steel connector for soldering application in automotive wire harness manufacturingMaterial Stainless steel connector 1.57” (40mm) long, 0.6” (15mm) OD & 0.4” (10mm) thick. Lead free solderTemperatur…
Date:2008/02/03
-
induction soldering led to aluminum housing
Soldering LED to aluminum housing Objective Heat an aluminum spotlight housing to solder an LED assembly to the inside baseMaterial LED housing with copper plug, aluminum spotlight housing 5” (127mm) dia at top, 1.25” (31.75mm) dia at base, temperature s…
Date:2008/02/03
-
induction soldering glass feedthroughs
Soldering Glass Feedthroughs Objective Heat a kovar fiber optic housing with glass feed-throughs to 400F (204.4C) within 20 seconds for a soldering application, to form a hermetic seal Material Kovar housing with 18 glass feed-throughs, solder preformsand …
Date:2008/02/03
-
induction soldering ferrule to fiber optic cable
Soldering Ferrule to Fiber Optic Cable Objective To heat a gold-plated ferrule and fiber optic cable to 475F within 8 seconds for a soldering applicationMaterial Gold-plated ferrule tube, fiber optic cable, solder preformTemperature 475 FFrequency 270 kHzE…
Date:2008/02/03
-
induction soldering fiber optic
Soldering Fiber Optic Objective To heat a fiber optic housing to 400F within 10 seconds for avsoldering application, to form a hermetic sealMaterial Gold-plated aluminum housing, solder preform ring and fluxTemperature 400 FFrequency 267 kHzEquipment Power…
Date:2008/02/03
-
induction soldering solar panel
soldering solar panel Objective Heat multiple joints on solar flex circuit strips to 500F (260C) within ten seconds for a soldering application.Material Flexible solar panel, Solder Plus Paste 63NC-A, 0.0625” (1.59mm) thick Teflon sheetsTemperature 500 F(…
Date:2008/02/03
-
induction soldering brass rings
Soldering brass rings Objective: To heat 1 3/4, 3 and 6 diameter brass slip rings and a sheathed copper wire assembly to 3600 F for soldering within three (3) to six (6) seconds. Currently production is accomplished by using a soldering iron and stick feed…
Date:2008/02/03
-
induction soldering brass bellows assembly
Soldering Brass Bellows Assembly Objective: To heat a brass bellows and end cap assembly to 450F for soldering within 20 seconds. Presently, a soldering iron is used to produce the joint between the bellows and cap. The customer requests a quality solder j…
Date:2008/02/03
-
induction soldering brass tubes
Soldering brass tubes Objective: Soldering two brass tubes measuring 3/4 and 1/4 together for use as cellular phone antennas. The lengths of tubes range from four (4) feet to twelve (12) feet, and must be soldered along the axial side. The joint is to be m…
Date:2008/02/03
-
induction soldering steel
Soldering Steel Objective To heat a special steel housing to 500(260) F(C) for a soldering applicationMaterial Steel housingSolder wire and fluxTemperature 500(260) 550(287.8) F(C)Frequency 200 kHzEquipment Power of 6kW, 150-400 kHz solid state induction …