induction brazing stainless steel joint
Objective Braze an end plug on a stainless steel joint of the car grill before powder coating application Material Stainless steel car grill 0.5” x 0.19” (12.7mm x 4.8mm), end plugs and braze ring Temperature 1350 F (732C) Frequency 267 kHz Equipment…
Date:2007/04/03
-
induction brazing stainless steel hose to copper elbow
Objective Braze a stainless steel braided hose to copper elbows for a braided hose assembly. Material Stainless steel braided hose 3/8” (9.5mm) OD, copper elbow 1/4” (6.3mm) OD, braze preform rings and black flux Temperature 1400 F (760 C) Frequency 2…
Date:2007/04/03
-
induction brazing two positions on a stainless steel manifold
Objective Simultaneously braze two positions on a stainless steel manifold Material Stainless steel manifold 4” (101.6mm) long, 1” (25.4mm) in diameter and nico braze Temperature 1800 F (982 C) Frequency 198 kHz Equipment • Power of 20kW induction h…
Date:2005/10/02
-
induction brazing steel-carbide tool
Objective Provide a solution to this steel-carbide brazing applicationMaterial • Body 10mm; carbide tip 57 x 35 x 3 mm• Braze shim• Braze flux whiteTemperature 750C (1382F)Frequency 152 kHzEquipment Power of 10kW induction heating system, equipped with …
Date:2005/10/02
-
induction brazing steel to steel
Objective To braze O-ring Face (ORFS) sleeve or male connector to a steel tube. Material • Steel tube, 1 inch (2.54 cm) OD • O-ring Face Seal sleeve and a male connector fittings • Preform braze rings • White SureFlow flux • Steel support mandrel…
Date:2005/10/02
-
induction brazing carbide to steel
Objective Braze a carbide sleeve to a steel ‘T’ shank Material 2.0” (51mm) OD carbide sleeve, 1.0” (25.5mm) high braze joint, 1.5 ” (38 mm) steel ‘T’ , 50% silver braze ring Temperature 1292 F (700 C) Frequency 257 kHz Equipment • Power of 10 k…
Date:2005/10/02
-
induction brazing stainless steel
Objective 1st Application: Braze hub assembly to needle holder 2nd Application: Braze Large tube to ring joint Material 1st Application: Steel hub assembly and needle 0.1” dia (2.5mm) 2nd Application: Steel tube 1” OD (25.4 mm) and ring Temperature 1…
Date:2005/10/02
-
induction brazing carbide teeth to steel pipe
Objective Brazing carbide teeth to a steel jaw in less than 5 minutes Material Steel pipe jaw, 0.5” (12.7mm) dia, 1.25” (31.75mm) long, 0.25” (6.35mm) thick carbide teeth, black flux and silver copper braze shims Temperature 1292F (700C) Frequency 25…
Date:2005/10/02
-
induction brazing carbide shaft to steel tube
Objective Braze a carbide shaft to a steel tube Material Carbide shaft 1/8” to 1” diameter (varying sizes) Steel tube 3/8” to 1 ” OD Silver solder braze Temperature indicating paint Temperature 1400 F for 60 seconds Frequency 220 kHz Equipment Pow…
Date:2005/10/02
-
induction brazing steel tube with copper ring
Objective To heat an oil suction assembly (steel tubing and filter cap) to 1,850F (1010C) within 15 seconds for a brazing application. Material 0.125” (3.2mm) diameter steel tube and filter cap assembly, high temperature brazing flux, copper ring. Tempe…
Date:2005/10/02