induction Annealing steel tubes
Objective To heat steel tubes to 2000 F (1093 C) in an inert atmosphere Material 0.1ā (2.54mm) diameter stainless steel tube Temperature 2000 F Frequency 333 kHz Equipment ā¢ 10 kW induction heating system, equipped with a remote workhead containingā¦
Dateļ¼2006/10/02
-
induction Annealing motor shaft
Objective Annealing the end of a steel hydraulic motor shaft prior to machining Material .75ā (19mm) diameter steel rod, 6ā (152.4mm) long with a keyway at the end Temperature 1350 F (732 C) Frequency 359 kHz Equipment ā¢ UM-06A-UHF induction heatingā¦
Dateļ¼2006/10/02
-
induction Annealing aluminum tubing
Objective Annealing aluminum fuel tank fill neck to 650 F (343 C) Material Aluminum fill neck 2.5ā (63.5mm) diameter, 14ā (35.5cm) long Temperature 650 F (343 C) Frequency 85 kHz Equipment ā¢ 40kW induction heating system, equipped with a remote workā¦
Dateļ¼2006/10/02
-
induction Annealing brass wire
Objective Continuously anneal a brass wire used in electric motors at a rate of 16.4 yds (15m) per minute to eliminate work hardening caused during the drawing process. Material Square copper wire 0.06ā (1.7mm) dia., temperature indicating paint Temperaā¦
Dateļ¼2006/10/02
-
induction Annealing aluminum lip
Objective Annealing a 1ā lip on aluminum cryogenic dewar that has been work hardened during the process of spin forming. Material Aluminum dewar, lip has a 3.24ā (82.3mm) ID and is 0.05ā (1.3mm) thick Temperature 800 F (427 C) Frequency 303 kHz Equiā¦
Dateļ¼2006/10/02
-
induction Annealing steel wire
Objective To heat 3ā (76.2mm) from the end of the wire on a woven wire cloth 60ā (1.52m) long. This prepares the wire mesh for bending in a press brake. Material Woven wire cloth (steel) made of 1/2ā (12.7) diameter wire, 60ā (1.52m) long. Wires are 1ā¦
Dateļ¼2006/10/02
-
induction Annealing copper tubing
Objective To heat both ends of a copper tube to anneal as soft as possible 1.5ā (38.1mm) from end and retain full hardness next to anneal Material 1.625ā (41.275mm) dia x 24ā (609.6mm) long copper tube Temperature 1500 F (815.5 C) Frequency 70 kHz Eā¦
Dateļ¼2006/10/02
-
induction Annealing brass crimping
Objective To anneal a small area of an electrical contact for crimpingMaterial Brass female spade electrical contact with single transverse loop at end 0.5Āh(12.7mm) long, 0.25Āh(6.3mm) wide and 0.03Āh (0.8mm) thick, 1000oF (538oC)heat paintTemperature ā¦
Dateļ¼2006/10/02
-
induction Annealing steel shaft
Objective Heating a steel rod to 1200F (649C) for an annealing, stress relief application Material 1.062ā (26.97mm) dia type T-410 stainless steel bar 6ā (1.82m) long & 1.25ā (31.75mm) dia T-416 stainless steel bar 6ā (1.82m) long Temperature 120ā¦
Dateļ¼2006/10/02
-
induction Annealing locknuts
Objective To heat locknuts to 2150F (1176C) for annealingMaterial Waspaloy locknutTemperature 2150F (1176C)Frequency 382 kHzEquipment ā¢ UM-10AB-UHF induction heating system, equipped with a remote workhead containing one 0.66Ī¼F capacitor.ā¢ An induction ā¦