Keywords"n"ļ¼total 3019 records
-
induction soldering brass rings
Soldering brass rings Objective: To heat 1 3/4, 3 and 6 diameter brass slip rings and a sheathed copper wire assembly to 3600 F for soldering within three (3) to six (6) seconds. Currently production is accomplished by using a soldering iron and stick feedā¦
Dateļ¼2008/02/03
-
induction soldering brass bellows assembly
Soldering Brass Bellows Assembly Objective: To heat a brass bellows and end cap assembly to 450F for soldering within 20 seconds. Presently, a soldering iron is used to produce the joint between the bellows and cap. The customer requests a quality solder jā¦
Dateļ¼2008/02/03
-
induction soldering brass tubes
Soldering brass tubes Objective: Soldering two brass tubes measuring 3/4 and 1/4 together for use as cellular phone antennas. The lengths of tubes range from four (4) feet to twelve (12) feet, and must be soldered along the axial side. The joint is to be mā¦
Dateļ¼2008/02/03
-
induction soldering steel
Soldering Steel Objective To heat a special steel housing to 500(260) F(C) for a soldering applicationMaterial Steel housingSolder wire and fluxTemperature 500(260) 550(287.8) F(C)Frequency 200 kHzEquipment Power of 6kW, 150-400 kHz solid state induction ā¦
Dateļ¼2008/02/03
-
induction soldering steel tube
Soldering Steel Tube Objective Heat a.125ā (3.175mm) diameter stainless steel tube to a 1ā diameter cylinder 1ā (25.4mm) tall for a soldering applicationMaterial Stainless steel cylinder and tubeTemperature indicating paint Lead free solder preform ringā¦
Dateļ¼2008/02/03
-
induction soldering copper
Soldering copper Objective Heat copper tab until the solder reflows. Material Copper tab 0.25 X 0.25 inch square about 0.05 inches thick. Lead free solder material (higher melting temperature than regular solder.) Temperature 500 F for 1.25 seconds ā¦
Dateļ¼2008/02/03
-
induction shrink fit cast iron
Shrink Fit Cast Iron Objective To use induction to prepare cast iron assemblies for shrink fit assemblyMaterial Customer supplied cast iron rocker arms of varying sizesTemperature 450 F (232 C)Process Time 20 secondsFrequency 48 kHzEquipment Power of 25kW,ā¦
Dateļ¼2008/02/03
-
induction shrink fit steel gear
Shrink fit steel gear Objective Heat the bore of a hardened spur steel gear to shrink fit onto a gear motor shaft. This is part of a chair for the disabled.Material Steel gear 2.5 h (63.5mm) OD, .75 h (19mm) ID x .625 h (16mm) thick, temperature indicatingā¦
Dateļ¼2008/02/03
-
induction shrink fitting carbide ring
Shrink fitting carbide ring Objective Shrink fitting a carbide ring into a steel valve seatMaterial Steel valve seat 6ā (152.4mm) OD with 3ā (76.2mm) ID hole & .75ā (19mm) thick, carbide ringTemperature 500 F ( 260 C)Frequency 55 kHzEquipment ā¢ Powā¦
Dateļ¼2008/02/03
-
induction shrink fitting impeller blades to shaft
Shrink fitting impeller blades to shaft Objective Heat aluminum impeller blades to 200 F (93 C) and shrink fit onto a shaft.Material Aluminum impeller blades with a .28ā (7.109mm) bore, aluminum shaftTemperature 200 F (93 C)Frequency 255 kHzEquipment ā¢ Pā¦
Dateļ¼2008/02/03