induction annealing steel tubes
Objective To heat steel tubes to 2000 F (1093 C) in an inert atmosphere Material 0.1ā (2.54mm) diameter stainless steel tube Temperature 2000 F Frequency 333 kHz Equipment ā¢ 10 kW induction heating system, equipped with a remote workhead containingā¦
Dateļ¼2006/10/02
-
induction annealing motor shaft
Objective Annealing the end of a steel hydraulic motor shaft prior to machining Material .75ā (19mm) diameter steel rod, 6ā (152.4mm) long with a keyway at the end Temperature 1350 F (732 C) Frequency 359 kHz Equipment ā¢ UM-06A-UHF induction heatingā¦
Dateļ¼2006/10/02
-
induction annealing aluminum tubing
Objective Annealing aluminum fuel tank fill neck to 650 F (343 C) Material Aluminum fill neck 2.5ā (63.5mm) diameter, 14ā (35.5cm) long Temperature 650 F (343 C) Frequency 85 kHz Equipment ā¢ 40kW induction heating system, equipped with a remote workā¦
Dateļ¼2006/10/02
-
induction annealing brass wire
Objective Continuously anneal a brass wire used in electric motors at a rate of 16.4 yds (15m) per minute to eliminate work hardening caused during the drawing process. Material Square copper wire 0.06ā (1.7mm) dia., temperature indicating paint Temperaā¦
Dateļ¼2006/10/02
-
induction annealing aluminum lip
Objective Annealing a 1ā lip on aluminum cryogenic dewar that has been work hardened during the process of spin forming. Material Aluminum dewar, lip has a 3.24ā (82.3mm) ID and is 0.05ā (1.3mm) thick Temperature 800 F (427 C) Frequency 303 kHz Equiā¦
Dateļ¼2006/10/02
-
induction annealing steel wire
Objective To heat 3ā (76.2mm) from the end of the wire on a woven wire cloth 60ā (1.52m) long. This prepares the wire mesh for bending in a press brake. Material Woven wire cloth (steel) made of 1/2ā (12.7) diameter wire, 60ā (1.52m) long. Wires are 1ā¦
Dateļ¼2006/10/02
-
induction annealing copper tubing
Objective To heat both ends of a copper tube to anneal as soft as possible 1.5ā (38.1mm) from end and retain full hardness next to anneal Material 1.625ā (41.275mm) dia x 24ā (609.6mm) long copper tube Temperature 1500 F (815.5 C) Frequency 70 kHz Eā¦
Dateļ¼2006/10/02
-
induction annealing brass crimping
Objective To anneal a small area of an electrical contact for crimpingMaterial Brass female spade electrical contact with single transverse loop at end 0.5Āh(12.7mm) long, 0.25Āh(6.3mm) wide and 0.03Āh (0.8mm) thick, 1000oF (538oC)heat paintTemperature ā¦
Dateļ¼2006/10/02
-
induction annealing steel shaft
Objective Heating a steel rod to 1200F (649C) for an annealing, stress relief application Material 1.062ā (26.97mm) dia type T-410 stainless steel bar 6ā (1.82m) long & 1.25ā (31.75mm) dia T-416 stainless steel bar 6ā (1.82m) long Temperature 120ā¦
Dateļ¼2006/10/02
-
electromagnetic induction and the joule effect
Induction Heating has the important characteristic that the heat is generated in the material to be heated itself. Principle of induction heatingBecause of this, induction has a number of intrinsic trumps, such as a very quick response and a good efficiā¦
Dateļ¼2006/10/02
© Copyright 2021. uihm.com All Rights Reserved.