Keywords"n",total 3019 records
-
induction brazing carbide to steel shaft
Objective Brazing a cone shaped carbide to a stainless steel shaft for a digger Material Cone shaped carbide 1.12” (28.4mm) dia, 1.5”(38.1mm) tall, stainless steel shaft 1.12” (28.4mm) dia and various length, black brazing flux and braze shims Tempera…
Date:2007/04/03
-
induction curing epoxy
Objective Heat the end of an aluminum copier roller to 400 F (200 C) to cure epoxyMaterial Aluminum roller 4.75” (120mm) diameter, 2’ (0.6m) long with 1.5” (38.1mm) thick plug at endTemperature 400 F (200 C)Frequency 52 kHzEquipment • Power of 25 kW in…
Date:2007/04/03
-
induction curing coating
Objective Curing a coating on both sides of an aluminum piston at a rate of 1” (25.4mm) per secondMaterial 4 aluminum pistons weighing 1lb (.45kg) each, 3.75” (95.25mm) dia and 2.5” (63.5mm) highTemperature 225 F (107.2 C)Frequency 6 kHzEquipment • Pow…
Date:2007/04/03
-
induction curing adhesive
Objective To Cure adhesive in aluminum filter endsMaterial Aluminum filter, steel end caps & plastisol adhesiveTemperature 200 FFrequency 277 kHzEquipment Power of 6kW induction heating system, equipped with a remote workhead containing two 0.1uF capa…
Date:2007/04/03
-
induction curing ceramic fiber
Objective To heat-cure a NextelTM Ceramic fiberMaterial Ceramic fiber 30,000 (9,145) ft(m) Steel tubeTemperature indicating paintTemperature 1300(700) F(C)Frequency 70 kHzEquipment Power of 45kW, 50-450 kHz solid-state induction power supply with a remote …
Date:2007/04/03
-
induction curing measuring tape paint
Objective To heat measuring tape stock at a maximum rate of 600 feet per minute to cure the applied paint. The heating coil is to accommodate the 3/8″ wide stock within the customer’s current framework. Curing must occur above 400F at the rate specified.…
Date:2007/04/03
-
induction bonding solar panels
Objective To heat the stainless steel substrate of a solar panel shingle in order to melt the polymer encapsulant, allowing two shingles to bond together with a 3 inch overlap. Material 3″ by 10.25″ section of a 21″ solar panel shingle Temperature 130…
Date:2007/04/03
-
induction bonding steel clips
Objective To heat metal clips and press-bond them into rubber seals. The metal needs to be heated to 250F to 350F with a cycle time not exceeding 3 seconds Material Steel clips and rubber sealer blocks Temperature 250F to 350F Frequency 373 kHz Equipme…
Date:2007/04/03
-
metal to plastic by induction bonding
Objective To heat a steel magnetic steel post to 300F for a bonding application.Material Magnetic steel posts Plastic handleTemperature indicating paintTemperature 300F (149C)Frequency 288 kHzEquipment Power of 6 kW, 100-400 kHz induction heating power sup…
Date:2007/04/03
-
induction annealing stress relieving
STRESS RELIEVING,NORMALISING AND ANNEALINGStress RelievingStress relieving is applied to both ferrous and non-ferrous alloys and is intended to remove internal residual stresses generated by prior manufacturing processes such as machining, cold rolling and…